Al Sb Cu Fe Pb Ni P Si S Sn Zn
Min/Max 0.005 0.5 82.0 - 85.0 0.2 7.0 - 9.0 1 0.5 0.005 0.08 7.0 - 9.0 0.8
Nominals - - 83.5000 - 8.0000 - - - - 8.0000 -
Product Type Temper Type
Continuous ASTM B505
Ingot ASTM B30
Sand ASTM B66
Temper Sect. Size Cold Work Type Min Temp Tensile Strength YS
0.05% UL
YS
0.02% Offset
YS
0.005% Offset
Elong. RH
B
RH
C
RH
F
RH
30T
VH
500
BH
500
BH
3000
Shear
Strgth
Fatigue
Strgth
Izod
Impact
Strgth
- in. % - F ksi ksi ksi ksi % B C F 30T 500 500 3000 ksi ksi ft-lb
- mm. - - C MPa MPa MPa MPa - - - - - - - - MPa MPa J
As Centrifugal Cast
M07 68 34 20 - - - - - - - - - - - -
M07 0 SMIN 20 234 138 - - 8 - - - - - - - - - 0
As Sand Cast
M01 68 32 16 - - - - - - - - - - - 15
M01 0 TYP 20 221 110 - - 20 - - - - - 60 - - 103 0
Product Property US Customary Metric
Coefficient of Thermal Expansion 10.0 . 10-6 per oF (68-392 F) 18.0 . 10-6 per oC (20-200 C)
Density 0.32 lb/in3 at 68 F 8.86 gm/cm3 @ 20 C
Electrical Conductivity 12 %IACS @ 68 F 0.07 MegaSiemens/cm @ 20 C
Electrical Resistivity 85.9 ohms-cmil/ft @ 68 F 14.29 microhm-cm @ 20 C
Modulas of Elasticity in Tension 11000 ksi 75800 MPa
Specific Gravity 8.86 8.86
Specific Heat Capacity 0.09 Btu/lb/oF at 68 F 377.1 J/kg . oK at 293 K
Thermal Conductivity 33.6 Btu . ft/(hr . ft2 . oF)at 68F 58.2 W/m . oK at 20 C
Joining Technique Suitability
Brazing Good
Coated Metal Arc Welding Not Recommended
Gas Shielded Arc Welding Not Recommended
Machinability Rating 70
Oxyacetylene Welding Not Recommended
Soldering Good
End Product Specification
Continuous ASTM B505
Ingot ASTM B30
Sand ASTM B66